POLYBOND is an
oxidized bitumen waterproofing membrane suitable for application by gas
torch or with hot bitumen, with a special multi-layered design for
superior pliability, tensile strength and workability. The
multi-layered design consists of a polyester core coated on both sides
with oxidized bitumen. The polyester core gives the membrane high
tensile strength, elongation and superior lap joint strength. Properly
installed POLYBOND forms an impervious waterproofing blanket
which accepts normal structural movement without breaking or cracking.
|
|
 
POLYBOND maybe used for wide
range of waterproofing applications including roofs, reservoirs,
basements, tunnels and car parks.
 
Excellent cost
performance ratio.
Good resistance to
fatigue and tear.
Outstanding bondability
and seam integrity.
Impact and puncture
resistant.
Single layer
installation reduces costs.
 
POLYBOND is installed by torch welding method, loose-laid
or fully bonded to substrate. When loose-laid, only laps are bonded
together. Peripheries and protrusions are sealed according to
specifications.

The underside of the membrane
should be torched just enough to superficially melt the bitumen.
Excessive heating may damage the reinforcement. Overlaps should be
reheated from the top and resealed with a trowel to ensure seam
integrity.For details of installation methods and flashing requirements,
consult the relevant BITUMAT Design and Installation Manual.
|
 Black
finish with thin, heat fusible polyethylene film on both surface.

|
For flat areas
|
1 mt.1.13 M2/M2
per layer
|
|
For 30 cm. girth flashing
|
0.35
M2/Mt/ length
|
|
Average wastage
|
3 - 5%
|
|
Average Weight
|
3,4 or 5kg/M2
|
 
POLYBOND complies with the requirements
of the tolerance levels of the following standards:
NF P 84314 Type 40 VV (France)
DIN 52131 V60 S4 (West Germany)..
 
In addition to stringent regular tests by BITUMAT
laboratory, our products are tested by Bureau Veritas &
SOCOTEC, Paris, France.
 
| Roll Length |
10mts |
| Roll width |
1 Mt. |
| Thickness |
3, 4 mm |
| Reinforcement |
50,60 gms glasfibre |
 
Gas torch, Knife, Trowel, Measuring tape, Marking string,
Gloves.
|
 |
 |
 |
| Softening point 0C |
115 + 5 |
ASTM D-36 |
| Penetration, @ 250C,
dmm |
20-35 |
ASTM D-5 |
| Low temperature
flexibility, 0C |
+5 to 0 |
UEAtc |
| Heat resistance,
compound stability @ 80 0C/2hr |
No flow - Pass |
UEAtc |
| Tensile strength,
N/5 Longitudinal
Transverse |
520
490 |
UEAtc. ASTM D-412
UEAtc. ASTM D-412 |
Elongation %
Longitudinal
Transverse |
40
50 |
ASTM D-412
ASTM D-412 |
Load strain prodcut
Longitudinal
Transverse |
20,800
24,500 |
CGSB-37-GP-56M
|
| Tear resistance, N
Longitudinal
Transverse |
120
110 |
UEAtc |
Puncture
Resistance, N Static indentation
Dynamic indentation |
L 3
l.3 |
ASTM E 154.
UEAtc 5.1.9
UEAtc 5.4.1 |
| Water Vapour
Permiability
Transmission (gm/M2 /24 hrs)
Permeance (perms) |
0.28
0.01 |
ASTM E-96 |
The information given in this Technical Sheet is to the best of our knowledge based on
laboratory tests and practical experience. However, as the product is often used under conditions beyond our control, we cannot guarantee but the product itself.
|